摘要: The interior shrinkage deformation and temperature change of high-strength concrete (HSC) at very early age, i.e., the first 24 h from casting, and up to an age of 72 h was investigated experimentally using optic fibre sensors (SOFO) and thermally sensitive resistors. The initial and the final setting times of HSC were also investigated. Results show that two turning points (I and II) on the development curve of deformation, both represent the onsets of the variation of rigidity in fresh HSC, can be recognized as the initial and the final setting times, which are evaluated around 4.5 h to 5.7 h and 9.0 h to 11.8 h, respectively. Also, the higher the fly-ash or silica fume replacement ratio, the longer the setting times. The setting times of HSC evaluated from the curve of temperature development are quite close to those measured from the deformation curve. In addition, the HSC setting times determined by penetration resistance method (ASTM C403) demonstrate unusually large values. This method is therefore not advised to be used to measure the setting times of HSC.
URI: http://hdl.handle.net/11455/70077
ISSN: 1023-2796
Appears in Collections:期刊論文

文件中的檔案:

取得全文請前往華藝線上圖書館



Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.